真空镀膜磁控溅射高压电源脉冲波形参数对薄膜附着力提升的影响

  Adhesion of a sputtered film depends on the energy with which the arriving atoms strike the substrate and on the cleanliness of the interface. The high voltage supply influences both, because it sets the target voltage that determines the sputter energy and, in a pulsed process, it sets the shape of the pulse that determines the ion flux during the interface cleaning step.

  A continuous direct current discharge is stable but tends to accumulate charge on insulating targets, and the accumulated charge produces arcs that eject particles and disrupt the film. A pulsed supply interrupts the discharge periodically, allowing the charge to neutralise during the off period, and the pulse parameters determine whether the neutralisation is complete. An off time that is too short leaves charge that produces a smaller arc at the next pulse; an off time that is too long allows the plasma to extinguish and the next pulse becomes an ignition transient with a high voltage overshoot.
  The pulse shape matters as much as the duty cycle. A pulse with a fast rise delivers high power during the initial part of the on period, which increases the instantaneous sputter rate and the energy of the arriving atoms, and that higher energy improves the interface mixing in the first few nanometres of film growth. The same pulse, applied after the film has grown, may damage the surface by resputtering. Programming the pulse shape to differ for the interface step and for the bulk step, therefore, is a practical way to get both adhesion and a smooth film.
  The off period is also the window for reactive gas control. In reactive sputtering the target is poisoned if the gas flow exceeds the rate at which it is consumed, and poisoning lowers the sputter rate and changes the film stoichiometry. Pulsing the discharge allows the gas to be admitted during the off period, when it is not immediately consumed, and to be consumed during the on period. The ratio of gas admitted to energy delivered becomes the control variable, and the supply must report the delivered energy per pulse accurately for that ratio to be held.
  Arc handling in a pulsed supply is a matter of speed. An arc on a poisoned target develops in a few microseconds and, if the energy is not removed quickly, leaves a crater that becomes a particle source for the rest of the run. A detection scheme that watches the voltage collapse and removes the drive within two microseconds, followed by a short off period and a controlled restart, is the standard approach. The restart must be soft, because a hard restart deposits a large energy in the arc region and can re-ignite the arc.
  Measurement of the pulse energy is not simple because the voltage and current are both changing during the pulse. A sampling scheme that multiplies instantaneous samples of voltage and current and integrates over the pulse gives the delivered energy, and the sampling rate must be high enough that the integration error stays below the tolerance. Integrating with a fixed interval that is short compared with the pulse width is adequate and simpler than a true analog multiplier.
  Adhesion testing closes the loop. A scratch test or a pull-off test on a coupon processed alongside the production parts gives a number that can be trended against the pulse parameters. When adhesion falls, the trend usually shows whether the interface cleaning step lost energy, which appears as a lower pulse energy during the first few seconds, or whether the bulk film changed, which appears as a different arc rate. Separating those two causes from the test data is possible when the pulse parameters are recorded per run.
  Chamber cleanliness sets a floor on the achievable adhesion. A chamber that has been used for a different material carries residues that contaminate the interface, and no pulse shaping compensates for that. A conditioning run with a getter target before a critical deposition is cheap insurance, and the pulse parameters for the conditioning run differ from the production run in that the energy is higher and the duration is shorter.
  Target erosion uniformity affects the film thickness distribution, which in turn affects the apparent adhesion in different regions. A magnetron whose erosion groove has deepened delivers less material at the centre, and the resulting thinner film adheres differently at the edges because the interface exposure time differs. Rotating the magnet or replacing the target on an erosion-based schedule keeps the distribution and the adhesion uniform across the substrate.
  Instrumentation should record the pulse waveforms rather than only their averages. A waveform library that stores one representative pulse per minute allows a change in shape to be detected even when the averages remain constant, and shape changes are often the first sign of a failing switch or a drifting gas composition.
  Pulse frequency selection has a practical constraint that is rarely stated: the frequency must not coincide with a mechanical resonance of the target assembly. A magnetron target is a heavy plate supported on a cooling structure, and its resonant frequencies lie in the range where pulsed supplies commonly operate. Driving the discharge at a frequency near a resonance produces a small vibration of the target, and the vibration modulates the gap between the target and the plasma, which modulates the discharge current and produces a beat in the film thickness. A frequency scan during commissioning, with an accelerometer on the target, identifies the resonances and allows the operating frequency to be chosen away from them.
  Gas composition control during a pulsed run is another item that is easy to get wrong. The pulsing changes the average consumption rate, and the controller that regulates the reactive gas sees a pulsing consumption that averages over the pulse period. If the controller bandwidth is higher than the pulse frequency it will try to follow each pulse and will oscillate; if it is much lower it will hold the average correctly. Setting the bandwidth below one tenth of the pulse frequency is the rule, and the gas valve should be sized so that the loop can still correct a step within a few seconds.
  Film thickness uniformity depends on the target-to-substrate distance and on the pressure, and both interact with the pulse parameters. A higher pressure scatters the sputtered atoms and improves uniformity at the cost of deposition rate, and a pulse that delivers more energy at the target raises the sputter rate, which partly compensates. Finding the combination that meets both the uniformity and the throughput specification is a matter of trials, and the trials should be recorded with the pulse parameters so the result can be reproduced.
  The supply's output filter has an influence on the arc behaviour that deserves mention. A large output capacitance stores energy that is delivered into the arc when it forms, which increases the damage. Keeping the capacitance small and the energy storage local to the switching stage reduces the arc energy, and the resulting supply responds faster to a fault. In a pulsed application the filter is usually small anyway, so the choice is consistent with the pulsing requirement.
  A supply whose output filter stores little energy and whose fault response is fast changes an arc from a crater source into an event that the next pulse recovers from, and that change is what keeps a long deposition run free of particles.
  Reactive gas control and pulse frequency interact through the target condition in a way that shows up as a slow oscillation in the film stoichiometry. A controller that is tuned for continuous operation will, under pulsing, correct on a timescale that coincides with the pulse period and produce a limit cycle. Detuning the controller, and adding a feed-forward term from the delivered pulse energy, removes the cycle and gives a stoichiometry that holds to a fraction of a percent over a run.
  A deposition run that ends with the target in a lightly poisoned state starts the next run from a different condition, which is why the first few minutes of a run often produce a film that differs from the rest. A short pre-sputter with the target clean, followed by the controlled transition into the production condition, makes the start reproducible and removes the need to discard the first wafers of a batch.
  Reproducibility begins with a target that starts each run in the same condition.
  A pulse library, a frequency scan during commissioning and a pre-sputter before each run are the three practices that make a sputtering process reproducible from batch to batch.
  A particle count taken after each run, recorded with the pulse parameters, gives a fourth data series that explains the failures the other three cannot, because a particle that appears without an arc event usually indicates a target that has begun to crack rather than a supply fault.
  A fourth data series taken after each run, and a monthly record of the pulse library, are the two practices that keep a sputtering process stable across a year of production.