Influence of Dynamic Impedance Matching of Etching Equipment High Voltage Power Supplies on High Aspect Ratio Trench Etch Rate
A deep trench etch is limited by the transport of ions and radicals to the bottom of a feature that becomes narrower as the etch proceeds, and the bias voltage at the wafer sets the ion energy that drives the transport. The load that the bias supply sees is a plasma sheath whose impedance changes as the trench deepens, and the change is large enough that a supply with a fixed output characteristic delivers a different voltage at the end of the etch than at the beginning.
The sheath behaves like a capacitor in series with a resistive path, and the effective capacitance depends on the sheath thickness, which depends on the voltage and the plasma density. At a high aspect ratio the ion flux to the wafer falls, the plasma density near the wafer changes, and the sheath capacitance moves. A supply that regulates the average voltage at the output terminal sees the sheath as a load that varies by tens of percent over a run.
The specification that captures this behaviour is the output impedance at the frequencies where the sheath varies. A supply with a low output impedance holds the wafer voltage through the variation; a supply with a high output impedance lets the voltage move with the load. Most specifications quote a load regulation figure measured on a resistor, and a resistor does not behave like a sheath.
Pulsed bias is the common way to control the ion energy distribution, and pulsing changes the matching problem. During the on phase the sheath is thin and the capacitance is high; during the off phase the sheath collapses and the load becomes nearly open. A supply that is matched for the on phase delivers a different waveform during the off phase, and the difference appears in the etch as a change of the ion energy distribution.
Dynamic matching in this context means the supply's control loop follows the load rather than the matching network following the frequency. The loop bandwidth has to be higher than the rate at which the sheath changes, which for a slow etch is tens of hertz and for a fast etch is a few hundred. A loop that is fast enough for the trench also amplifies the plasma's own noise, which is the trade that has to be settled by measurement rather than by rule.
Reflected energy is a symptom rather than a cause. In a bias supply that drives a sheath through a cable, the reflection at the cable to sheath transition produces a standing wave whose amplitude depends on the mismatch. The standing wave changes the voltage at the wafer without changing the voltage at the supply terminal, and a measurement taken at the terminal underestimates the wafer's exposure.
The measurement point matters more than the measurement accuracy. A voltage probe at the supply terminal reads a value that is the sum of the wafer voltage and the drop across the cable and the blocking capacitor. At high aspect ratio the wafer voltage is the quantity that sets the etch rate, and the probe location has to be as close to the electrode as the design allows. A probe mounted on the electrode, with a defined attenuation and a defined bandwidth, is worth the effort.
Wafer temperature is coupled to the bias through the ion flux. A higher bias draws more ion current, which heats the wafer, which changes the etch chemistry, which changes the rate. The chuck's cooling holds the temperature only if the electrostatic clamping is adequate, and the clamping voltage is another supply whose stability affects the etch. Two supplies that are specified separately can interact through the wafer temperature in a way that neither specification predicts.
Arcs in the chamber are normal events and the bias supply has to survive many such events. An arc draws a current that is limited by the sheath and by the supply's own impedance, and the arc energy that reaches the electrode is what damages the wafer. A supply that interrupts within a few microseconds keeps the energy below the damage threshold, and a supply that limits rather than interrupts lets the arc persist until the plasma recovers.
Process drift over a run is the effect that operators notice first. A trench that is 10 percent shallower at the end of a run than at the beginning is usually attributed to polymer buildup, and the bias voltage drift is a second candidate that is rarely measured. Recording the wafer voltage through the run, with the same probe used for qualification, separates the two causes.
High aspect ratio features are sensitive to the voltage waveform in a way that the average value does not describe. The ion energy distribution depends on the instantaneous voltage during the on phase, and a waveform with a slow rise delivers a broader energy distribution than a square wave. The distribution affects the bottom corner profile, and the profile is what the process specification measures.
Maintenance of the bias path is mostly about the blocking capacitor and the cable. A capacitor whose capacitance has fallen produces a higher voltage at the electrode for the same supply setting, and the etch rate rises until the process drifts out of specification. A cable whose dielectric has absorbed moisture produces a leakage path that shifts the voltage and adds noise. Both are measured during a maintenance window with the chamber vented.
Commissioning a bias supply for trench work ends with a rate test at two aspect ratios. The voltage that produces the target rate at a shallow feature is not the voltage that produces the target rate at a deep one, and the difference is the load dependence that the specification has to capture. Two points measured once are worth more than a curve computed from a model.
The blocking capacitor is a component whose value matters more than the specification sheet suggests. A capacitor that is too small produces a voltage droop during a long pulse, and the droop reduces the ion energy at the end of the pulse. A capacitor that is too large passes the low frequency components of the plasma noise into the supply, and the supply's protection sees a disturbance that is not a fault.
Cable length between the supply and the electrode is a parameter that should be fixed at installation and recorded. A cable that is longer than the design value adds inductance that slows the current rise during an arc, which sounds helpful and delays the protection's response to the arc. The two effects nearly cancel, and the protection timing that was validated on the bench no longer matches the installed machine.
Arc detection on the bias supply is easier when the detection is on the derivative of the current rather than on the magnitude. A plasma that is being driven hard has a current with a large reactive component, and a magnitude threshold that clears the reactive component is far above the arc current. A derivative threshold sits between the normal rate and the arc rate and catches the arc within a microsecond.
Wafer clamping and bias interact through the same electrode. The clamping voltage and the bias voltage are superimposed, and a clamping supply that is slow to settle leaves the electrode at an intermediate potential while the bias is being established. The etch that happens during that interval sees a different ion energy, and the first few seconds of a step are therefore a separate process condition.
Process qualification usually fixes the bias setting and varies the time. The rate at a fixed voltage falls as the aspect ratio rises, and the fall is the physics rather than a fault. A qualification that measures the rate at two times and extrapolates assumes a constant rate, and the assumption is wrong for any feature deeper than a few microns.
The supply's behaviour during a step change is part of the process recipe. A step from one bias level to another that takes longer than the gas settling time produces a period where the chemistry and the energy are both in transition, and the transition leaves a visible band in the profile. Faster steps reduce the band and stress the supply, and the usable step time is found by looking at the profile rather than at the voltage trace.
Service records for a bias supply should include the wafer voltage measured at the probe, not only the supply's own reading. The difference between the two readings grows as the cable and the blocking capacitor age, and the growth is the early sign of a component that will eventually fail. A difference trend is more useful than a single difference measurement.
The electrode's surface condition changes the sheath in a way that is easy to mistake for a supply problem. An electrode with a polymer film left from a previous run has a different secondary electron emission, the sheath potential shifts, and the voltage measured at the probe changes for the same setting. Cleaning the electrode restores the reading, and the shift is often attributed to a drifting supply until the cleaning is done.
Gas chemistry changes the load faster than any other variable in the chamber. A step that switches from a fluorine rich chemistry to an oxygen rich one changes the sheath thickness within a second, and a supply that is regulating the average voltage moves the wafer voltage by several percent. The etch that follows the step runs at the wrong energy for the first second, and the first second is a measurable fraction of a short step.
The fault that most often defeats a bias supply's protection is a slow arc rather than a fast one. A slow arc grows over tens of microseconds, and a detector that looks for a fast edge misses the growth. A detector that looks at the current's rate and at the voltage's collapse together catches the slow arc, and the combination is what a production machine needs.
Documentation of the bias path should include the measured voltage at the electrode for a set of standard conditions. When the machine is serviced, the same conditions are repeated, and the comparison shows whether the path has changed. A file with one number per condition is more useful than a paragraph describing the circuit.
The supply's output filter has a frequency response that the process can excite. A filter that is tuned to reject the switching ripple also has a resonance at a lower frequency, and a step change in the plasma can excite the resonance into a ringing that lasts tens of milliseconds. The ringing appears in the wafer voltage and in the etch, and the filter's damping is the parameter that fixes the ringing.
Training the operators on the bias supply is mostly about recognizing the difference between a process change and a hardware change. A rise in etch rate with the same settings is a hardware sign; a rise with different settings is a process sign. The distinction is cheap to teach and expensive to learn by trial.
Recipes are written in volts and read by the plasma in amps.